Hastelloy C-22 C22 Alloy C22 UNS N06022 2.4602 NiCr21Mo14W Forged Forging Rings Rolled Rings Forging Sleeves Bushes Bushing Pipes Piping tubes tubings barrels Casing Cases Shells cylinders hubs housin
型号:
parameters1:
parameters2:
parameters3:
parameters1:
parameters2:
parameters3:
We are professional Hastelloy C-22 C22 Alloy C22 UNS N06022 2.4602 NiCr21Mo14W Forged Forging Rings Rolled Rings Forging Sleeves Bushes Bushing Pipes Piping tubes tubings barrels Casing Cases Shells cylinders hubs housings Parts Pieces Material Products from china
Chemical Composition
C | Mn | P | S | Cr | Mo | Si | V | Co | W | Fe | Ni | ||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
2.4602 | Min % | 20,00 | 12,50 | 2,50 | 2,00 | bal. | |||||||
Max % | 0,01 | 0,50 | 0,025 | 0,015 | 22,50 | 14,50 | 0,08 | 0,35 | 2,50 | 3,50 | 6,00 | bal. | |
(Key to Steel 2010) | |||||||||||||
alloy 22 N 06022 | Min % | 20,00 | 12,50 | 2,50 | 2,00 | remainder. | |||||||
Max % | 0,015 | 0,50 | 0,020 | 0,020 | 22,50 | 14,50 | 0,08 | 0,35 | 2,50 | 3,50 | 6,00 | remainder | |
ASTM B622 |
Physical properties
Property | Value |
---|---|
Density: lb/in3 | 0,314 |
Hardness: HB | 240( max) |
Permeability at 20°C/68°F | < 1,001 |
Temperature T °C/F (°C/F) | Specific heat J / kgK (Btu / lb °F) | Thermal conductivity W/mK (Btu·in / ft2·h·°F) | Electric resistance µΩ · cm (Ω circ mill / ft) | Modulus of elasticity kN/mm2 (103 ksi) | Expansion rate from 70°F bis T 10-6 / K (10-6 / °F) |
---|---|---|---|---|---|
100 / 212 | 423 (--) | 11,1 (--) | 123 (--) | 202 (--) | 12,4 (--) |
200 / 393 (204 /400) | 444 (0,106) | 13,4 (94) | 124 (746) | 197 (28,4) | 12,4 /(6,9) |
300 / 572 316 / 600 | 460 (0,119) | 15,5 (111) | 125 (753) | 190 (27,6) | 12,5 (7,0) |
400 / 752 (427 / 800)( | 476 (0,114) | 17,5 (131) | 126 (759) | 185 (26,2) | 13,1 (7,4) |
500 / 932/ (538 / 1000) | 495 (0,117) | 19,5 (140) | 127 (767) | 178 (25,7) | 13,7 (7,7) |
600 / 1112 (649/ 1200) | 514 (0,125) | 21,3 (156) | 128 (774) | 173 (24,8) | 14,3 (8,1) |
700 / 1292 (760 /14009 | 533 | 23,2 | 129 | 167 (23,6) | 14,9 (8,5) |
800 / 1472 (871 / 1600) | 159 (22,3) | 15,5 (8,8) | |||
1000 / 1832 | 143 (20,7) | 16,2 |
Mechanical properties (20°C / 68°F)
Yield strengthRp0,2 min.N/mm2/ ksi | 310/ 45 | ||
---|---|---|---|
Yield strength1,0 min. N/mm2/ksi | 335 /49 | ||
Tensile strength Rm N/mm2/ ksi | 690 /100 | ||
Elongation A 5 ( %) | 45 | ||
ISO V-notch impact toughness (Avarage values at RT ) j/cm2 | >=150 | ||
ISO V-notch impact toughness (Avarage values at(-196°C) -320°F) j/cm2 | >=120 |